Cured-in-place pipe (CIPP) has been widely used in pipeline rehabilitation as a trenchless, environmentally friendly and efficient repair technology. A three-dimensional computational model of the mechanical response of ring-fractured pressure pipe lining under bending moment is established by the finite element method, and the established model is verified by using the results of existing literature. The effects of parameters such as internal pressure, bending moment, outer diameter of the liner, liner thickness and friction coefficient between the liner and the host pipe on the stress of the liner are analyzed. The results show that: When the internal pressure exceeds 0.6 MPa, the maximum stress of the liner pipe is concentrated at the top of the ring section, and its radial displacement is only 0.24%~0.97% of the maximum displacement of the host pipe, indicating that the increase in internal pressure can effectively suppress the relative deformation of the liner and the host pipe. The length of the pipe section that generates stress in the liner increases linearly with the bending moment, outer diameter and thickness, but is suppressed by the internal pressure and friction coefficient. For example, when the friction coefficient increases from 0.1 to 0.6, the length of the pipe section that generates stress in the liner is shortened by about 30%, which provides a quantitative basis for the parameter trade-off in the design. At the circumferential position θ=90°, the stress on the inner surface of the liner exceeds that on the outer surface, and the difference becomes significant as θ increases.
Wang Kaidong
,
Fang Hongyuan
,
Hu Deqiang
,
Li Bin
,
Zhai Kejie
. Mechanical Response of the Liner in a Ring-Fractured Pressure Pipe under Bending Moments[J]. Chinese Journal of Underground Space and Engineering, 2026
, 22(4)
: 1400
-1410
.
DOI: 10.20174/j.JUSE.2026.04.28
[1] 王威,许星星,侯本伟,等.跨断层埋地管道基于性态的抗震设计参数研究[J].应用基础与工程科学学报, 2023, 31 (2):400-412. (Wang Wei, Xu Xingxing, Hou Benwei, et al. Study on performance-based seismic design parameters of buried pipelines crossing fault[J]. Journal of Basic Science and Engineering, 2023, 31 (2):400-412. (in Chinese))
[2] 曾成,冯涵璐,王仁超.基于原型监测与数值计算的管道边坡灾害安全评估与分析[J].水利水电技术(中英文), 2024, 55(4): 36-47. (Zeng Cheng, Feng Hanlu, Wang Renchao. Pipeline slope disaster safety evaluation and analysis based on in-situ monitoring and numerical calculations[J]. Water Resources and Hydropower Engineering, 2024, 55(4): 36-47. (in Chinese))
[3] Zhang Y D, Wong R C. Effect of corrosion on buried pipe responses under external load: experimental and numerical study [J]. Tunnelling and Underground Space Technology, 2023, 132:104934.
[4] Peter J M, Chapman D, Moore I D, et al. Impact of soil erosion voids on reinforced concrete pipe responses to surface loads [J].Tunnelling and Underground Space Technology, 2018, 82:111-124.
[5] Zhai K J, Fang H Y, Wang N N, et al. Mechanical behavior of pressure pipe rehabilitated by CIPP liner under reverse fault [J]. Journal of Earthquake Engineering, 2025, 29(6):1227-1240.
[6] Zhai K J, Chen Q, Fang H Y, et al. Mechanical response of the pressure pipeline rehabilitated by polymer liner under the action of surface load [J]. Journal of Pipeline Science and Engineering, 2025:100289.
[7] Zhai K J, Wang K D, Hu D Q, et al. Mechanical behavior of prestressed concrete cylinder pipe strengthened by prestressed CFRP subject to secondary load[J]. Advances in Structural Engineering, 2025,28(11):2117-2130.
[8] 马保松编. 非开挖工程学 [M]. 北京:人民交通出版社; 2008. (Ma Baosong. Trenchless engineering[M]. Beijing: China Communications Press, 2008. (in Chinese))
[9] 马保松编. 非开挖管道修复更新技术 第2版 [M]. 北京:人民交通出版社, 2024. (Ma Baosong. Trenchless pipeline rehabilitation and revewal technology [M]. Beijing: China Communications Press, 2024. (in Chinese))
[10] Matthews J. Sewer rehabilitation using an ultraviolet-cured GFR cured-in-place pipe [J]. Practice Periodical on Structural Design and Construction, 2015, 20(1):04014021.
[11] 杨寅昌,黄志伟,全学友,等.地下管线非开挖修复技术国内外应用现状[J].地下空间与工程学报, 2024, 20(增2): 1021-1027. (Yang Yinchang, Huang Zhiwei, Quan Xueyou, et al. Application status of trenchless repair technology of underground pipeline at home and abroad[J]. Chinese Journal of Underground Space and Engineering, 2024, 20(Supp.2): 1021-1027. (in Chinese))
[12] 郑玉,郑世华.非开挖紫外光固化技术在砖涵修复中的应用[J].地下空间与工程学报, 2020, 16(增2): 812-817.(Zheng Yu, Zheng Shihua. Application of trenchless UV curing technology in the repair of brick culvert[J]. Chinese Journal of Underground Space and Engineering, 2020, 16(Supp.2): 812-817. (in Chinese))
[13] Allouche E N, Bainbridge K, Moore I D. Laboratory examination of a cured in place pressure pipe liner for potable water distribution system[J]. North American Society for Trenchless Technology, 2005, 1.
[14] Brown M J,Fam A, Moore I D. Material characterization of components and assembled behavior of a composite liner for rehabilitation of cast iron pressure pipes [J]. Polymer Engineering and Science, 2008, 48(7):1231-1239.
[15] Brown M J, Moore I D, Fam A. Performance of a cured-in-place pressure pipe liner passing through a pipe section without structural integrity [J]. Tunnelling and Underground Space Technology, 2014, 42:87-95.
[16] ASTM. Standard Specification for Cured-in-Place Pipe Lining System for Rehabilitation of Metallic Gas Pipe(F2207-06(2019))[S]. 2019.
[17] Adebola T, Moore I D, Hoult N. Use of optical fibers to investigate strength limit states for pressure pipe liners spanning across circular perforations [J]. Journal of Pipeline Systems Engineering and Practice, 2021, 12(2):04021006.
[18] Brown M J, Moore I D,Fam A. Analysis of a cured-in-place pressure pipe liner spanning circular voids [J]. Tunnelling and Underground Space Technology, 2020,101:103424.
[19] ASTM. Standard Practice for Rehabilitation of Existing Pipelines and Conduits by the Inversion and Curing of a Resin-Impregnated Tube (F1216-16)[S]. 2016.
[20] Fu G Y, Shannon B, Deo R, et al. An equation for hole-spanning design of underground cast iron pipes lined with polymeric liners [J]. Tunnelling and Underground Space Technology, 2022,123:104435.
[21] US-AWWA. Journal AWWA - Legislation/Regulation -- Inside Senate Bill (AWWA JAW36183)[S]. 1994.
[22] Moore I D. Response of a polymer liner passing across a pressure pipeline joint opening under axial ground movements [J]. Computers andGeotechnics. 2021, 139:104429.
[23] Fu G Y, Shannon B, Azoor R, et al. Equations for gap-spanning design of underground cast iron pipes lined with thermosetting polymeric liners [J]. Tunnelling and Underground Space Technology, 2022, 119:104234.
[24] Zhai K J, Moore I D. Axial stresses in pressure pipe liners spanning joints with initial gap, opening as a result of differential ground movements [J]. Tunnelling and Underground Space Technology, 2023, 133:104965.
[25] Zhai K J, Moore I D. Bending response and design equations for gravity-flow pipe liners passing across ring fractures or joints [J]. Journal of Pipeline Systems Engineering and Practice, 2024, 15(4):04024043.
[26] Zhai K J, Fang H Y, Wang N N, et al. A simplified solution for buried continuous pipe rehabilitated by liner under the effect of surface load and soil void[J]. Canadian Geotechnical Journal, 2025,62: 1-15.
[27] Lan H T, Hoult N, Moore I D. Numerical investigation of strain variations along steel pipelines in four-point bending tests [J]. Journal of Pipeline Systems Engineering and Practice, 2024, 15(4):04024042.