Hydration Heat Effects in Cut-and-Cover Tunnel Structures under Different Casting Methods

  • Xu Ping ,
  • Liu Wei ,
  • Chen Bin ,
  • Qiao Biao ,
  • Kang Weiwei
Expand
  • 1. School of Civil Engineering, Xiangtan University, Xiangtan, Hunan 411105, P. R. China;
    2. Key Laboratory of Geotechnical Mechanics and Engineering Safety of Hunan, Xiangtan University, Xiangtan, Hunan 411105, P. R. China;
    3. China Railway Seventh Bureau Group Co., Ltd., Guangzhou Engineering Company, Guangzhou 510700, P. R. China

Received date: 2025-10-24

  Online published: 2026-09-29

摘要

为探究大体积混凝土明洞隧道结构在水化热作用下的开裂敏感性及分布特征,以广湛高铁机场明洞隧道工程为背景,采用现场监测与数值模拟相结合的方法,研究了底板-拱墙间隔浇筑与连续浇筑两种方式下的混凝土水化热效应及抗裂性能。结果表明:两种浇筑方式下,混凝土表层防裂安全系数均低于1.15,为潜在开裂敏感区域。连续浇筑条件下,开裂敏感区域主要分布于混凝土表层,隧道整体最小防裂安全系数为0.34;间隔浇筑条件下,开裂敏感区域不仅分布于混凝土表层,还在拱墙养护阶段出现于拱脚处底板内部,其底板与拱墙的最小防裂安全系数分别为0.43和0.49。两种浇筑方式的差异主要集中于底板-拱墙接触区域,间隔浇筑在养护阶段该区域防裂安全系数低于1.15,而连续浇筑该区域大于1.15且隧道整体性更好,但其防裂安全系数最小值较间隔浇筑略有降低。总体而言,连续浇筑虽在一定程度上整体降低了防裂安全系数最小值,但提高了拱脚处底板内部的防裂安全系数最小值,致使潜在开裂敏感区域主要集中于混凝土表层。在此情况下,通过针对性加强表面防裂措施即可有效控制裂缝发展,并有利于缩短施工工期。研究成果可为类似工程的浇筑方案选择及温控防裂设计提供参考。

本文引用格式

徐平 , 刘惟 , 陈宾 , 乔彪 , 康炜炜 . 不同浇筑方式下明洞隧道结构水化热效应研究[J]. 地下空间与工程学报, 2026 , 22(S1) : 203 -212 . DOI: 10.20174/j.JUSE.2026.S1.23

Abstract

To investigate the crack sensitivity and its spatial distribution of mass concrete cut-and-cover tunnel structures under hydration heat, the airport cut-and-cover tunnel of the Guangzhou-Zhanjiang High-Speed Railway was selected as the case study. A combined approach of field monitoring and numerical simulation was employed to examine the hydration heat effects and anti-cracking performance under two casting methods:staged casting of the invert and arch wall, and continuous casting. The results indicate that, under both casting methods, the anti-cracking safety factor of the concrete surface is lower than 1.15, identifying it as a potential crack-sensitive zone. Under continuous casting, crack-sensitive regions are mainly distributed in the concrete surface layer, and the minimum anti-cracking safety factor of the entire tunnel structure is 0.34. Under staged casting, crack-sensitive regions occur not only at the surface but also within the invert near the arch springing during the arch wall curing stage, with minimum safety factors of 0.43 and 0.49 for the invert and arch wall, respectively. The differences between the two casting methods are primarily concentrated at the invert-arch wall interface:under staged casting, the safety factor in this region is lower than 1.15 during curing, whereas under continuous casting it exceeds 1.15 and the overall structural integrity is improved; however, the minimum safety factor of the structure is slightly lower than that of staged casting. Overall, although continuous casting slightly reduces the global minimum anti-cracking safety factor, it increases the minimum safety factor within the invert near the arch springing, resulting in potential crack-sensitive regions being mainly concentrated at the concrete surface. Under such conditions, effective crack control can be achieved by implementing targeted surface crack prevention measures, while also shortening the construction period. The findings of this study can provide a reference for the selection of casting schemes and the design of temperature control and crack prevention in similar engineering projects.

参考文献

[1] 王铁梦著. 工程结构裂缝控制 第2版[M]. 北京:中国建筑工业出版社,2017.
[2] Singh M P,Sen S, Pathak H, et al. Early age cracking relevant to mass concrete dam structures during the construction schedule[J]. Construction and Building Materials, 2024, 411:134739.
[3] Do T A, Hoang T T, Bui-Tien T, et al. Evaluation of heat of hydration, temperature evolution and thermal cracking risk in high-strength concrete at early ages[J]. Case Studies in Thermal Engineering, 2020, 21:100658.
[4] Zhao Y, Li G, Fan C, et al. Effect of thermal parameters on hydration heat temperature and thermal stress of mass concrete[J]. Advances in Materials Science and Engineering, 2021, 2021(1):5541181.
[5] Liu D, Zhang W, Tang Y, et al. Prediction of hydration heat of mass concrete based on the SVR model[J].Ieee Access, 2021, 9:62935-62945.
[6] Zhang Y, Wang S, He S, et al. Analysis of factors influencing the temperature field variation in mass concrete during hydration heat release[J]. Case Studies in Thermal Engineering, 2023, 52:103737.
[7] 李志鹏,罗奇星,韩庆华,等.大体积混凝土墙水化放热温度场分析[J].天津大学学报(自然科学与工程技术版),2023,56(8):878-885.
[8] 杨新浩,张凌云,董军,等.承台现浇大体积混凝土温度效应及影响参数分析[J].混凝土,2025(3):12-19+23.
[9] 汪建群,魏桂亮,刘杰,等.跨海大桥大体积混凝土承台水化热实测与分析[J].桥梁建设,2020,50(3):25-31.
[10] 杨益波,郭智渊,韩炜,等.基于水化热抑制剂的大体积混凝土温控技术[J].科学技术与工程,2024,24(19):8227-8238.
[11] Zhu J, Wang Z. Experimental modeling and quantitative evaluation of mitigating cracks in early-age mass concrete by regulating heat transfer[J]. Journal of Building Engineering, 2024, 96:110641.
[12] Sheng X, Xiao S, Zheng W, et al. Experimental and finite element investigations on hydration heat and early cracks in massive concrete piers[J]. Case Studies in Construction Materials, 2023, 18:e01926.
[13] Wang S,Duan J, Zhang Y, et al. Optimization of cooling system parameters with temperature field of mass concrete during hydration[J]. Case Studies in Thermal Engineering, 2024, 64:105456.
[14] 杨新浩,董军,张凌云,等.大体积混凝土承台分次浇筑层间水化热效应的相互影响研究[J].公路,2025,70(3):156-163.
[15] 吕国儿,汤群益,王定仕,等.大体积混凝土水化热损伤计算方法[J].河海大学学报(自然科学版),2024,52(4):29-34.
[16] 王思纯,廖宜顺,万世辉.不同温度下矿渣对铝酸盐水泥早期水化行为的影响[J].硅酸盐通报,2022,41(4):1343-1351, 1368.
[17] 王新刚.大体积混凝土温度应力实用计算方法及控裂工程实例[M]. 北京:人民交通出版社,2017.
[18] 王东海,张宏,王雅.桩基对大体积承台水化热问题影响研究[J].混凝土,2020(3):44-48, 53.
[19] 中华人民共和国住房和城乡建设部.大体积混凝土施工标准(GB 50496—2018)[S].北京:中国建筑工业出版社,2018.
文章导航

/

〈 〉