本文针对压气储能地下洞室柔性密封材料在恒温老化与循环拉伸作用下力学性能和渗透特性变化的问题,以丁基橡胶为研究对象,开展了循环拉伸加载与恒温热老化试验,系统研究了不同循环次数与温度条件下材料拉伸强度、拉断伸长率及气体渗透系数的演变规律。试验结果表明:随着应变循环次数增加,柔性密封材料的拉伸强度、渗透性降低,拉断伸长率升高,同时发现了丁基橡胶1 500次应力循环前后力学性能的不同。而在恒温老化作用下,随着温度水平的上升,柔性密封材料的力学性能有所下降,但不影响密封层的使用性能,65 ℃恒温老化作用对密封层的渗透影响较小,而80 ℃尤其是100 ℃时渗透性有较为明显的上升,所以压气储能洞室需尽量控制最高温度。
This study addresses the changes in mechanical properties and permeability characteristics of flexible sealing materials for underground compressed air energy storage (CAES) caverns under cyclic tensile loading and constant-temperature thermal aging. Using butyl rubber as the research subject, cyclic tensile tests and constant-temperature thermal aging experiments were conducted to systematically investigate the evolution of tensile strength, elongation at break, and gas permeability coefficient under different numbers of cycles and temperature conditions. The experimental results indicate that as the number of strain cycles increases, the tensile strength and permeability of the flexible sealing material decrease, while the elongation at break increases. Additionally, differences in the mechanical properties of butyl rubber before and after 1500 stress cycles were observed. Under constant-temperature aging, as the temperature level rises, the mechanical properties of the flexible sealing material decline, though this does not affect the usability of the sealing layer. Aging at 65°C has a minimal impact on the permeability of the sealing layer, whereas at 80 ℃ and especially at 100 ℃, permeability increases significantly. Therefore, it is essential to control the maximum temperature in CAES caverns as much as possible.
[1] 夏才初,周舒威,周瑜,等.压缩空气储能的地下岩石内衬洞室关键技术[M].上海:同济大学出版社,2021.
[2] Jiang Z, Li P, Tang D, et al. Experimental and Numerical Investigations of Small-Scale Lined Rock Cavern at Shallow Depth for Compressed Air Energy Storage[J].Rock Mechanics and Rock Engineering, 2020, 53(8):1-13.
[3] Ma Y, Rao Q, Huang D, et al. A new theoretical model of local air-leakage seepage field for the compressed air energy storage lined cavern[J]. Journal of Energy Storage, 2022(May):49.
[4] 周小松,闫磊,黄康康,等.圆形截面隧道式储气库群布局参数研究[J].地下空间与工程学报, 2024, 20(S01):205-212.
[5] 孙冠华, 易琪, 于显杨,等. 压缩空气储能电站大罐式地下内衬硐库上覆岩体稳定性分析[J]. 中国科学:技术科学, 2024, 54 (12):2377-2391.
[6] 周瑜, 夏才初, 周舒威,等. 压气储能内衬洞室高分子密封层的气密与力学特性[J]. 岩石力学与工程学报, 2018, 37 (12):2685-2696.
[7] Suryatal B, Phakatkar, Rajkumar K, et al. Fatigue Life Estimation of an Elastomeric Pad by ε-N Curve and FEA[J].Journal of Surface Engineered Materials and Advanced Technology, 2015, 05(2):85-92.
[8] Zaghdoudi M, Koemmling A, Boehning M, et al. Ageing of elastomers in air and in hydrogen environment:A comparative study[J].International journal of hydrogen energy,2024(Apr.):63.
[9] Tomer N S, Delor-Jestin F, Singh R P, et al. Cross-linking assessment after accelerated ageing of ethylene propylene diene monomer rubber[J]. Polymer Degradation & Stability, 2007, 92(3):457-463.
[10] Zhao F, Ren Z, Wu H, et al. Improved thermal oxidative aging resistance of silicone rubber via incorporation with Fe-MOFs[J]. Polymer Testing, 2026, 155109096-109096.
[11] Pawar V, Pant R, Guruprasad P. Experimental and numerical studies on the effect of elongation rate and temperature on the mechanical behaviour of high strength NBR[J]. Plastics, Rubber and Composites, 2019, 48(7):13.
[12] Qin S, Xia C, Zhou S, et al. Airtightness of a flexible sealed compressed air storage energy (CAES) tunnel considering the permeation accumulation of high-pressure air[J]. Journal of Energy Storage, 2024, 84.
[13] 黄远红, 张凯, 梅军, 等.丁基橡胶密封材料的老化研究[J]. 润滑与密封, 2009, 34(7):6.
[14] Kim H M, Rutqvist J, Ryu D W, et al. Exploring the concept of compressed air energy storage (CAES) in lined rock caverns at shallow depth:A modeling study of air tightness and energy balance[J]. Applied Energy, 2012, 92:653-667.
[15] Takagi S, Nishimoto Y. Application of Air-Tight Sheet in the Storage Tank for the Generation of Electricity by the Compressed Air Energy Storage Gas Turbine System (CAES-G/T)[J]. Geosynthetics Engineering Journal, 2009:308-317.
[16] 刘宇艳,万志敏,田振辉,等. 单向聚酯帘线增强橡胶材料疲劳特性研究[J]. 复合材料学报, 1998, (4):99-103.
[17] 张帆, 张力伟, 熊英,等. 温度和疲劳共同作用对溴化丁基橡胶气体阻隔性能的影响[J]. 高分子材料科学与工程, 2024, 40 (2):134-140.
[18] 刘琼, 刘晓丹, 尹文华. 氟橡胶在寿命评估时压缩永久变形、压缩应力松弛与气密性关系的研究[J]. 合成材料老化与应用, 2023, 52 (6):46-48.
[19] Du Pont M, Costello J R. The Effects of Strain History on the Permeability of Polymers. Journal of Polymer Science Part B:Polymer Physics, 1996, 34(8):1423-1432.
[20] Pocius A, Schwarz M. Permeability Changes in Rubber Due to Stress Cycling[J]. Rubber Chemistry and Technology, 1988, 61(3):409-421.
[21] 莫一婷,杨林德,伍振志,等.遇水膨胀橡胶的老化性能试验研究及寿命预测[J].地下空间与工程学报, 2009, 5(2):5.
[22] 张力伟. 高阻隔溴化丁基橡胶耐疲劳性能研究[D]. 成都:四川大学,2021.